Environmental Science & Technology· Huang·· 8 天前AI 评分38

酸-rich ZSM-5 调控富电子 Cu–O–Ce 位点实现抗碱/重金属中毒的高效脱硝

Zeolite-Regulated Electron-Rich Cu–O–Ce Sites for Efficient Denitrification against Alkali/Heavy Metal Poisoning

AI 导读

设计 CuCeOx/ZSM-5 催化剂,利用富酸 ZSM-5 向 CuCeOx 转移电子生成富电子 Cu–O–Ce 位点,在 180–410 °C 范围内 deNOx 效率超过 90%(T90 = 180–410 °C)。

AI 深度导读基于原文整理的分节解读
背景
在碱金属和重金属中毒条件下,催化剂难以维持宽温度窗口的脱硝活性,这是环境催化领域待解决的问题。
做法
设计CuCeOx/ZSM-5催化剂,用富酸沸石调控富电子金属位点,使强酸位与Cu–O–Ce活性位接触,考察其NH3–SCR温度窗口与抗K/Pb中毒能力。
结论
富酸界面促进电子从ZSM-5向CuCeOx转移,生成富电子Cu–O–Ce位点,兼具反应物吸附活化与抑制NH3氧化作用;该催化剂在180–410 °C内脱硝效率>90%。K主要通过降低表面酸性和促进低活性硝酸盐积累使催化剂失活,Pb则通过诱导Cu2+→Cu+转化并占据CeO2氧空位,抑制Ce4+→Ce3+还原;中毒后T90仍为230–380 °C。
意义
工作给出碱金属与重金属离子使NH3–SCR催化剂失活的两条路径,并提出面向复杂烟气的高性能抗中毒催化剂设计思路;摘要未交代长期稳定性与实际烟气验证。

原文摘要

出版方登记 · Crossref

Enhancing the wide-temperature-window deNOx activity of catalysts under alkali/heavy metal poisoning conditions remains a pivotal challenge in the field of environmental catalysis. To tackle this issue, we designed a novel CuCeOx/ZSM-5 catalyst using an acid-rich zeolite-modulated electron-enriched metal site strategy. This strategy enables the contact between strong acid sites and Cu–O–Ce active sites, simultaneously regulating the efficient NH3–SCR temperature window and enhancing K/Pb poisoning resistance. Compared to CuCeOx, the engineered acid-rich interface significantly facilitates electron transfer from ZSM-5 to CuCeOx, generating electron-rich Cu–O–Ce active sites. These sites not only serve as adjacent adsorption and activation centers for reactants but also inhibit NH3 oxidation, and CuCeOx/ZSM-5 catalyst achieves >90% deNOx efficiency over a wide temperature range of 180–410 °C (T90 = 180–410 °C). K deactivates the catalyst mainly by reducing surface acidity and promoting the accumulation of less-reactive nitrate species, while Pb primarily suppresses Ce4+ → Ce3+ reduction via inducing Cu2+ → Cu+ conversion and occupying CeO2 oxygen vacancies. Notably, the poisoned CuCeOx/ZSM-5 catalyst still retains satisfactory deNOx performance, with the T90 = 230–380 °C. This work not only provides novel mechanistic insights into the deactivation pathways of NH3–SCR catalysts by alkali and heavy metal ions but also offers a viable strategy for the rational design of high-performance, poisoning-tolerant NH3–SCR catalysts tailored for complex flue gas environments.

页面未能读取全文,以上为出版方登记的摘要;方法与图表见原文

本页是 AI 精读,不转载论文原文;完整论文(含方法、图表与参考文献)见原文

来源:Environmental Science & Technology · doi.org