溶剂/阴离子共耗尽溶剂化工程构建低配位电解液,使 6.8 Ah 钠离子软包电池在 −20 °C 保持 162 Wh kg–1
Solvent/Anion Codepleted Solvation Engineering Enables Low-Coordination Electrolytes for High-Energy and Low-Temperature Sodium-Ion Pouch Cells
Journal of the American Chemical Society 论文报告,一种通过溶剂/阴离子共耗尽溶剂化工程构建的低配位电解液,使 6.8 Ah 钠离子软包电池在 25 °C 达到 200 Wh kg–1,并在 −20 °C 保持 162 Wh kg–1。
- 背景
- 钠离子电池要同时做到高能量密度和低温可靠运行,但一直受制于一个难以兼顾的矛盾:高压下正极与电解液界面的稳定性,与低温下的离子传输动力学,很难同时满足。原文把这一矛盾作为出发点,将调控电解液的溶剂化结构作为突破口,希望得到一种既能支撑高电压、又不牺牲低温动力学和离子电导的电解液。这一思路的难点在于:溶剂与阴离子各自与 Na+ 的配位都要被削弱,但削弱过度又会影响盐的溶解与离子输运。
- 做法
- 作者提出“溶剂与阴离子共贫化”的溶剂化工程,通过一种体积大、缺电子的添加剂 TMSB(tris(trimethylsilyl)borate)介导的竞争性阴离子络合,构建低配位电解液。按原文描述,TMSB 优先与 PF6– 络合,从而抑制阴离子与 Na+ 的直接配位;其大位阻骨架同时打断常规的离子对网络,并限制溶剂与 Na+ 的过度配位,由此把电解液的配位环境整体“拉低”。围绕这一设计,作者测了离子电导率与去溶剂化能垒,表征了正极-电解液界面(CEI)的模量与成分,并把电解液与 NFM、NVP、P2-NNMO 三种正极匹配,在最高 4.5 V、−40 至 25 °C 的条件下考察兼容性,最后把体系放大到 6.8 Ah 软包电池评级。
- 结论
- 关键量化结果按原文给出的顺序如下:离子电导率由 2.41 mS cm–1 提升到 5.34 mS cm–1;去溶剂化能垒由 44.82 kJ mol–1 降到 33.97 kJ mol–1。所生成的 CEI 模量达 2.7 GPa,且为无机物富集型。电解液在 NFM、NVP、P2-NNMO 三种正极上均表现出兼容性,电压上限到 4.5 V,温度窗口覆盖 −40 至 25 °C。放大后的 6.8 Ah 软包电池在 25 °C 下给出 200 Wh kg–1,原文称这一能量密度为创纪录水平;在 −20 °C 下仍保持 162 Wh kg–1。
- 机制
- 性能提升来自配位环境改变这条因果链:TMSB 对 PF6– 的优先络合减少了阴离子与 Na+ 的直接接触,位阻骨架又阻断离子对网络、抑制溶剂对 Na+ 的过量配位,于是 Na+ 的配位程度降低,离子传输更顺畅,去溶剂化所需越过的能垒也随之下降到 33.97 kJ mol–1。界面侧的贡献则来自阴离子分解形成的无机物富集、高模量(2.7 GPa)CEI:它一方面缓解正极表面退化,另一方面抑制正极材料的体相相变。
- 意义
- 这项工作的产出是一套可迁移的分子设计思路,而不是单一配方:通过一种大位阻缺电子添加剂同时实现溶剂贫化与阴离子贫化,把电导率、去溶剂化能垒和界面稳定性三件事放进同一个调控手段里。三种正极、4.5 V 上限、−40 至 25 °C 的兼容性数据,加上 6.8 Ah 软包电池 200 Wh kg–1(25 °C)和 162 Wh kg–1(−20 °C)的结果,说明该策略在极端环境储能方向上具备放大潜力。
原文摘要
出版方登记 · CrossrefWidespread deployment of sodium-ion batteries demands both high energy density and reliable low-temperature (LT) operation, but is constrained by a persistent trade-off between high-voltage stability (cathode/electrolyte) and LT ion-transport kinetics. Herein, we report a solvent/anion codepleted solvation engineering strategy to construct low-coordination electrolytes through competitive anion complexation mediated by a bulky electron-deficient additive, TMSB (tris(trimethylsilyl)borate). We reveal that TMSB preferentially complexes with PF6– to suppress direct anion-Na+ coordination, while its bulky steric backbone disrupts conventional ion-pair networks and restricts excessive solvent-Na+ coordination. This strategy fundamentally boosts ionic conductivity (from 2.41 to 5.34 mS cm–1) and lowers the desolvation energy barrier (from 44.82 to 33.97 kJ mol–1). Moreover, such a strategy enables a high-modulus (2.7 GPa), inorganic-rich cathode-electrolyte interphase (CEI), which can not only mitigate surface degradation, but also suppress bulk phase transitions of cathode materials. Consequently, the electrolyte demonstrates broad compatibility across diverse cathodes (NFM, NVP, and P2-NNMO) under extreme voltage (up to 4.5 V) and temperature (−40 to 25 °C) conditions. Remarkably, the scaled-up 6.8 Ah pouch cell achieves a record-high energy density of 200 Wh kg–1 at 25 °C, while maintaining 162 Wh kg–1 even at −20 °C, offering a generalizable molecular paradigm for extreme-environment energy storage.
页面未能读取全文,以上为出版方登记的摘要;方法与图表见原文
本页是 AI 精读,不转载论文原文;完整论文(含方法、图表与参考文献)见原文
这种低配位电解液设计让 6.8 Ah 钠离子软包电池在 −20 °C 仍保持 162 Wh kg–1,可作为低温钠离子电池电解液开发的分子层面设计参考。
来源:Journal of the American Chemical Society · doi.org