Advanced Energy Materials· Tian·· 8 天前AI 评分64

竞争配位深共晶电解质使 LiCoO2 软包电池实现 5000 次循环

Competitive Solvation Structure in a Deep Eutectic Electrolyte Enables High‐Voltage LiCoO 2 ‐Based Pouch Cells With 5000‐Cycle Stability

AI 导读

一种以 succinonitrile(SN)和 dimethyl sulfone(MSM)构建的深共晶电解质(DEE)将 Li+ 溶剂化结构从聚集体(AGGs)调节为 AGGs 与接触离子对(CIPs)的均衡分布,离子电导率为 3.87 mS cm−1,Li+ 迁移数为 0.81。

AI 深度导读基于原文整理的分节解读
背景
富阴离子溶剂化结构能改善界面稳定性,但常阻碍Li+去溶剂化,从而限制高电压锂金属电池的快充与低温性能。常规做法是使用高浓度电解液或弱溶剂化电解液,本文提出另一条路径:用深共晶电解液(DEE)来实现溶剂化结构的调控。
做法
电解液由丁二腈(SN)与二甲基砜(MSM)构成,两者具备竞争配位能力。这种竞争把Li+溶剂化从聚集体(AGGs)为主转向AGGs与接触离子对(CIPs)的均衡分布,从而降低Li+去溶剂化能垒、提升传输动力学,使DEE的离子电导率达到3.87 mS cm−1、Li+迁移数为0.81。MSM的作用是缓和SN的过度配位、抑制负极副反应,使锂沉积/剥离稳定持续6800 h。在此基础上引入LiTFSI/LiDFOB双盐体系进一步优化界面化学,形成由无机富集内层与柔性有机外层构成的双层固态电解质界面。
结论
LiCoO2||Li电池在5C、3.0–4.5 V条件下循环1000次后容量保持97.1%,并可在−10°C下稳定运行。3.0 Ah的LiCoO2||Li软包电池能量密度达到417 Wh kg−1;LiCoO2||石墨软包电池则实现超过5000次循环的长期耐久性。
意义
结果说明,通过SN与MSM的竞争配位调节溶剂化结构,可在不依赖高浓度或弱溶剂化路线的前提下同时兼顾动力学与界面稳健性,为高电压、快充型深共晶电解液的设计提供了一种可操作的配方思路,并已在软包电池层面得到验证。

原文摘要

出版方登记 · Crossref

Anion‐rich solvation structures improve interfacial stability but often impede Li + desolvation, limiting fast‐charging and low‐temperature performance in high‐voltage lithium metal batteries. Unlike conventional high‐concentration or weakly solvating electrolytes, we propose a deep eutectic electrolyte (DEE) using succinonitrile (SN) and dimethyl sulfone (MSM) with competitive coordination capability. This design shifts the Li + solvation from aggregate clusters (AGGs) to a balanced AGGs/contact ion pairs (CIPs) distribution, which lowers the Li + desolvation energy barrier, enhances the transport kinetics, and endows the DEE with an ionic conductivity of 3.87 mS cm −1 and a Li + transference number of 0.81. MSM moderates excessive SN coordination, suppressing parasitic reactions on the anode, thereby enabling stable Li plating/stripping for 6800 h. A lithium bis(trifluoromethanesulfonyl)imide (LiTFSI)/lithium difluoro(oxalato)borate (LiDFOB) dual‐salt system further optimizes interfacial chemistry, yielding a bilayer solid electrolyte interphase comprising an inorganic‐rich inner layer and a flexible organic outer layer. LiCoO 2 ||Li cells retain 97.1% capacity after 1000 cycles at 5C (3.0–4.5 V) and operate stably at −10°C. A 3.0 Ah LiCoO 2 ||Li pouch cell further delivers a high energy density of 417 Wh kg −1 , and LiCoO 2 ||graphite pouch cells sustain long‐term durability over 5000 cycles. This competitive solvation strategy effectively harmonizes kinetics and interfacial robustness for high‐voltage, fast‐charging DEEs.

页面未能读取全文,以上为出版方登记的摘要;方法与图表见原文

本页是 AI 精读,不转载论文原文;完整论文(含方法、图表与参考文献)见原文

来源:Advanced Energy Materials · doi.org