低温介导层状胶束组装制备具取向孔道和高互联性的皱褶介孔碳纳米球
Low-Temperature-Mediated Lamellar–Micelle Assembly of Wrinkled Mesoporous Carbon Nanospheres with Aligned Pores and High Interconnectivity
一种 5 °C 低温层状胶束组装策略制得孔径 36 nm、比表面积 315 m2 g–1、孔道互联度达 96% 的皱褶介孔碳纳米球,结果发表于 Journal of the American Chemical Society。其钠存储负极在 10 A g–1 下达 142 mAh g–1,2 A g–1 循环 1000 次保持 90.5%。
- 背景
- 介孔材料的孔道是否通透,直接决定扩散有多快。问题在于,真正把孔道做成直通、高互连的可控手段一直很有限:现有介观结构大多来自球状胶束组装,得到的是曲折孔道。作者把这一现状作为出发点,想绕开球状胶束,找一条能长出发散状、高互连介孔的组装路径,并用它来应对与扩散相关的应用需求。
- 做法
- 关键做法是更换组装单元,而非改动配方配比。作者用共聚物 L121/F127 复合体系构建层状胶束,取代常规球状胶束,并让其在沉降的 F127 晶种上发生异相生长,温度控制在 5 °C;作者把低温与层状胶束这两点列为控制这种非寻常组装的关键。所得褶皱介孔碳纳米球在去除模板后粒径约 910 nm、比表面积 315 m2 g–1、孔径均一在 36 nm,径向介孔通道的互连度最高达 96%。作者还调节反应温度与模板比例,以改变孔径和褶皱程度,显示这条路线存在可调的参数窗口。材料随后被用作钠存储负极,并以商业硬碳作为对照来考察倍率与循环表现。
- 结论
- 去模板后的碳球同时具备大孔径与高互连:孔径均一在 36 nm,互连度最高 96%,比表面积 315 m2 g–1,粒径约 910 nm。电化学方面,径向排列的大孔结构在 10 A g–1 下给出 142 mAh g–1 的倍率容量;在 2 A g–1 下循环 1000 圈后容量保持 90.5%。这两项结果是在与商业硬碳对比的语境下给出的。此外,孔径与褶皱程度可随反应温度和模板配比调节,说明结构参数并未被单一点位锁死。
- 机制
- 作者的解释分两层。在组装层面,用层状胶束而非球状胶束,是形成发散状、高互连径向介孔的原因,这也是该体系与传统介孔碳在结构上的分界。在性能层面,径向对齐的大孔结构使电荷传输和电解液渗入更顺畅,作者据此把倍率与长循环的表现归因于孔道几何,而不是碳骨架本身的其它性质。
- 意义
- 这条路线提供的是一套组装模式,而不仅是一个介孔碳配方:用层状胶束构建介孔高速通道,且孔径与褶皱程度可由温度、模板比例调节。对于依赖快速扩散的场景,例如作者示例中的钠存储负极,径向大孔、96% 互连的球形颗粒把“孔道怎么排布”变成了一个可以在合成端设计的变量。
原文摘要
出版方登记 · CrossrefMesoporous structures with highly permeable channels are of great significance for fast diffusion; however, the delicate engineering of straightforward pores remains quite limited, with most of mesostructures are tortuous pores derived from spherical micelle assembly. Herein, we explore a novel lamellar–micelle assembly approach that enables to generate a type of wrinkled mesoporous carbon nanospheres with highly interconnected divergent mesopores. In place of the conventional spherical micelles, the key for controlling such unusual assembly is determined by the construction of laminar micelles (copolymer L121/F127 composite) and heterogeneous growth on sedimented F127 seeds at a low temperature of 5 °C. The fabricated wrinkled mesoporous carbon nanospheres after template removal possess a particle size at ∼910 nm, a high surface area of 315 m2 g–1, a uniform pore size at 36 nm, as well as radial mesochannels with high interconnectivity up to 96%. Further regulation on the reaction temperature and template ratio allows for a high tunability over the pore size and wrinkle degree. When employed as a sodium storage anode, the radially aligned large-pore structure drastically facilitates charge transport and electrolyte penetration, thus delivering rate capability (142 mAh g–1 at 10 A g–1) and long-term cyclability (90.5% retention after 1000 cycles at 2 A g–1) compared to commercial hard carbon. Our work underscores a particular assembly pathway through lamellar micelles as an effective approach for building up ultrafast mesopore highways toward promising diffusion-related applications.
页面未能读取全文,以上为出版方登记的摘要;方法与图表见原文